Metal restoration
Metal ReSurfacer
Brings architectural metal and anodised aluminium back to its natural sheen without stripping the protective coating. Takes out stage 1 and 2 corrosion. It will not take out pitting.
- Coverage
- 250 to 500 sq ft / quart
- Removes
- Stage 1 and 2 corrosion
- Clean the pad
- 3 to 6 times / hour
- Respirator
- Dust mask required
Order
Metal Resurfacer Case
$669.95You will also need
On corrosion this is a machine process, and it runs on the same pad and backer as the glass system. For very light staining a rag or a white non-abrasive pad is enough.
- ReSurfacer Pad 6in$21.60
- Backer Pad 6in$23.90
- Variable speed polisher or random orbital sanderNot supplied
Not sure how much the job takes? Work it out below
Before you start
This product carries no signal word on its safety data sheet, which is why its info chart reads User Friendly: Yes. It is water based and acid-free. The hazard here is the dry dust, and the risk to the work is a contaminated pad.
What to know
- A fine particle dust mask is required. Take precautions against inhaling the dry dust from this product.
- It will not remove pitting. It takes out the beginning stages of corrosion. Once the metal is pitted, that is physical loss of material and no polish puts it back.
- Every metal behaves differently and this has been tested on most but not all. Test an area first, and examine the test in direct sunlight from several angles.
- Never let dirt or sand touch the pad or the product. Never let the pad or the polisher touch the ground. Circular scratch patterns mean the pad is contaminated.
- Plug the polisher into a ground fault interrupter, since you are working with electricity and water together.
- Professional use only, by qualified technicians. Consulting and training are available from Presto.
Required protection
- Fine particle dust mask
- Ground fault interrupter on the polisher
- Painters masking tape for the working area
Where this sits in the metal system
Restore the metal, then protect it. Restoring anodised aluminium and leaving it bare is how the oxidation comes straight back.
Step 1 · Clean · often enough
EnviRestore MSR
For staining rather than corrosion. If the metal is dirty rather than damaged, start here before reaching for a polisher.
View productStep 2 · Restore · you are here
Metal ReSurfacer
250 to 500 sq ft per quart. Stage 1 and 2 corrosion, oxidation, ion exchange, water erosion, scratches, etching and chemical burns, taken back to the natural sheen without damaging the protective coating.
Step 3 · Protect
Metal Protector
Seals the restored metal and preserves the restoration investment. There are two grades, and they cover very different areas per quart, so read both before ordering.
View Metal Protector MDIt shares the glass system's hardware. The same ReSurfacer Pad and Backer Pad used for glass restoration drive this product too, so a crew already set up for glass needs no new equipment to take on metal.
How to apply it
- 1
Mix it and test it
Shake or stir the product well before use. A small amount covers a large area. Test on an inconspicuous patch first and examine it in direct sunlight from several angles before committing to the elevation.
- 2
Light staining, by hand
In many cases no polisher is needed. Apply a small amount with a white synthetic non-abrasive pad and agitate the surface until the stain lifts, using water to keep the surface lubricated. A rag or microfiber towel is enough for very light staining.
- 3
Aggressive stains, by machine
Put a small amount on the ReSurfacer Pad, filling the holes in the pad, which are there to hold the product. Run the polisher at medium speed so the product does not spray off onto other surfaces, pressing firmly on the metal until the stain is gone. Suction cups let a technician brace themselves or the swing stage so real pressure can be applied.
- 4
Keep it moist, aim for a milky paste
Keep the working surface wet with a spray bottle of water, preferably deionised. The consistency you want is a milky paste. It should not drip down the surface and it should not cake on the pad. Getting the balance right takes experimentation on each job, and that balance is where the product's full potential is.
- 5
Clean the pad 3 to 6 times an hour
Dry buffing cakes the product and clogs the pad, which slows everything down. Run the polisher upside down on slow and work a stainless steel or copper wire brush from the centre of the pad outward, then rinse with the spray bottle and carry on. Performance is best immediately after cleaning. If the work slows or stops, clean the pad.
- 6
Watch for contamination
Stop frequently to check for scratching. Never let the pad or polisher touch the ground or any dusty surface. Circular pattern scratches mean the pad or the product has picked up contamination, and the answer is to clean the pad.
Equipment needed
- ReSurfacer Pad
- ReSurfacer Backer Pad
- Variable speed polisher or random orbital sander
- Spray bottle
- Cleaning bucket and brush
- Microfiber towels
- Painters masking tape
- Small particle dust mask
- Ground fault interrupter and electrical cord
Work faster
Have everything to hand so the work is continuous. A small bottle of product in a pocket or on a tool belt, and a spray bottle attached to the technician, means the pad never has to leave the metal while water or product is added.
A random orbital sander instead of a variable speed polisher reduces the chance of scratching, but takes longer and may not clear heavily stained metal.
Technical details
| Coverage | 250 to 500 sq ft per quart |
|---|---|
| Sold as | 1 quart bottle, or a 12 quart case |
| Solvent | Water based |
| Flammable | No |
| User friendly | Yes no signal word on the safety data sheet |
| Economically efficient | Yes |
| Environmentally friendly | Yes |
| Acid free | Yes, and contains no harsh abrasives |
| Colour | White |
| Smell | None |
| Suitable surfaces | Architectural metal and anodised aluminium |
| Removes | Stage 1 and 2 corrosion, oxidation, ion exchange, surface scratches, water erosion, etching, chemical and acid burns, acid rain, mineral deposits including silicates, calcium, lime, magnesium, rust, salts and efflorescence, soap scum, oils, adhesive stains, water repellent overspray and leaching, caulking and coating residue, exhaust fumes and everyday buildup |
| Will not remove | Pitting |
| Pad cleaning | 3 to 6 times per hour |
Warranty terms in full
The information provided by Presto for the safe and effective use of this product, and all of our products, is believed to be good and accurate. However, due to the many different possible applications of this product, careful consideration should be made when selecting its suitability for each surface.
The information provided should never be substituted for individual testing to ensure the compatibility of the product with each surface intended for use. The purchaser shall assume all responsibility for determining the suitability of this product. When used as intended, this product will perform as stated. No other warranty can be made for this product, verbally or in writing.
Presto warrants this product to be free from defects. In the event this product is found to be defective, we will provide a sufficient amount of product to replace the defective product.